Abstract

Antimony and bismuth can both alloy with up to three molar equivalents of lithium and are therefore attractive candidates for replacing graphite in Li-ion battery anodes. Li3Sb and Li3Bi have the same cubic structure (Fm3 ̅m), but the ternary Li-Sb-Bi system has not been studied. We synthesized Li3(SbxBi1-x) with different Sb mole fractions at room temperature by ball-milling. These ternary alloys all have cubic crystal structures, as determined by XRD, but show a tendency towards phase segregation for x = 0.25 and 0.50. For x = 0.25, the lattice parameter presents a clear positive deviation from Vegard’s law in XRD, while for x = 0.50, XRD reveals two phases after milling, with the Bi-rich minority phase diminishing after thermal annealing. Solid-state nuclear magnetic resonance spectroscopy provides evidence for a Sb-enriched environment around the Li atoms for Li3Sb0.25Bi0.75, and nuclear spin-lattice relaxation measurements of the binary and ternary alloy phases point to low activation energies and rapid Li ion diffusion in Li3Bi.

Keywords

Anodes
Solid state NMR
Dynamics
Mechanochemical synthesis
Lithium ion batteries

Comments

Comments are not moderated before they are posted, but they can be removed by the site moderators if they are found to be in contravention of our Commenting Policy [opens in a new tab] - please read this policy before you post. Comments should be used for scholarly discussion of the content in question. You can find more information about how to use the commenting feature here [opens in a new tab] .
This site is protected by reCAPTCHA and the Google Privacy Policy [opens in a new tab] and Terms of Service [opens in a new tab] apply.