Degradation of high molar mass poly(ethylene glycol), poly(2-ethyl-2-oxazoline) and poly(vinyl pyrrolidone) by reactive oxygen species

31 August 2017, Version 1
This content is a preprint and has not undergone peer review at the time of posting.

Abstract

The development of the apparent molar mass of different poly(ethylene glycol), poly(2-ethyl-2-oxazoline) and poly(vinyl pyrrolidone) upon incubation with hydrogen peroxide and different concentrations and catalytic amounts of CuSO4 was followed used gel permeation chromatography.

Keywords

polymer degradation
reactive oxygen species
gel permeation chromatrography
oxidative degradation
biomaterials
polymer stability
hydrogen peroxide
Chemistry

Comments

Comments are not moderated before they are posted, but they can be removed by the site moderators if they are found to be in contravention of our Commenting Policy [opens in a new tab] - please read this policy before you post. Comments should be used for scholarly discussion of the content in question. You can find more information about how to use the commenting feature here [opens in a new tab] .